Material comparison

Basalt, E-glass, carbon and asbestos across seven criteria, with the source of each range.

Basalt fiberE-glassCarbon fiberAsbestos
Sort by

Health & safety

Fibre respirability and handling

Basalt fiberLow risk
E-glassModerate
Carbon fiberLow risk
AsbestosHigh risk

Tensile strength

Material-level typical value

Basalt fiber4,840 MPa
E-glass3,450 MPa
Carbon fiber4,900 MPa
Asbestos3,000 MPa

Elastic modulus

Material-level typical value

Basalt fiber90 GPa
E-glass76 GPa
Carbon fiber230 GPa
Asbestos160 GPa

Electrical insulation

Dielectric behaviour

Basalt fiberNon-conductive
E-glassNon-conductive
Carbon fiberConductive
AsbestosNon-conductive

Alkali resistance

Strength retention in alkaline exposure

Basalt fiber≥ 90 %
E-glass≈ 60 %
Carbon fiber≈ 95 %
Asbestos≈ 100 %

Heat resistance

Continuous service window

Basalt fiber650 °C
E-glass380 °C
Carbon fiber400 °C
Asbestos500 °C

Cost efficiency

Indicative, depends on grade and volume

Basalt fiber1.0×
E-glass0.9×
Carbon fiber8.0×
Asbestos0.6×

Bar length is a relative score on material-level typical values, not a tested guarantee.

How to read it

Four conclusions that survive a specification review.

Stiffness is the difference

Basalt sits above E-glass on typical modulus, which matters in deflection-controlled designs such as bridge deck and pultruded profiles.

Carbon buys stiffness at cost

Carbon is the stiffest option and the most expensive. Where the design is not stiffness-critical, the premium rarely returns its value.

Asbestos is the cautionary case

Heat resistance is high, but respirable fibre is a health hazard and is restricted in most markets. It is not a substitute candidate.

Alkali resistance decides concrete

In cementitious and marine exposure, strength retention in alkaline conditions separates a viable reinforcement from a short-lived one.

Typical ranges behind the bars

PropertyBasaltE-glassCarbon
Tensile strength3,000–4,840 MPa2,000–3,500 MPa3,000–7,000 MPa
Elastic modulus85–100 GPa72–76 GPa230–600 GPa
Continuous service−260~650 ℃−60~350 ℃−60~400 ℃
Density2.6–2.8 g/cm³2.5–2.6 g/cm³1.7–1.9 g/cm³
Alkali retention≥85 %LowerHigh
Electrical insulation介电介电导电

Ranges are material-level references for direction, not acceptance values. Delivered values follow the technical agreement.

Next step

Run the three-step selector, then request a sample against the returned specification.

Bar length is a relative score on material-level typical values, not a tested guarantee.

Reply within 24 hours on business days

Request a sample