03 — Composite products
Basalt Fiber Composite Rebar
About one quarter the weight of steel rebar, no corrosion path.
Standards
- GB 50608-2020
- GB/T 26743-2011
- GB/T 26745-2011
- JT/T 776.4-2010
- JG/T 351-2012
- T/CHTS 10025-2020

≥1200 MPa
vs ≥570 MPa HRB400
1.8–2.2
Steel 7.85
≥85 %
Typical value
Overview
Pultruded and wound from high-strength basalt continuous fiber with epoxy or unsaturated resin. A non-corroding reinforcement for road, bridge, tunnel, port and marine structures.
Core benefits
Light
Strong
Stable
Efficient
Technical parameters
| Parameter | Value |
|---|---|
| Density | 1.8–2.2 g/cm³ |
| Tensile strength | ≥1200 MPa |
| Tensile modulus | 45–55 GPa |
| Compressive strength | ≥500 MPa |
| Shear strength | ≥150 MPa |
| Elongation at break | >2 % |
| Thermal expansion (L / T) | 6–12 / 21–22 ×10⁻⁶/℃ |
| Acid retention | ≥80 % |
Typical values. Contractual values are confirmed by the mill test report and the technical agreement.
Applications
Send the specification and the operating condition — we reply with data, not adjectives.
Request a quoteRelated products
View allSee the data first. Then talk price.